I have a lipbalm kettle with stainless steel pipes that get up to 160deg when workers pour more lipbalm in kettle it cause the pipes to cool off enough that lipbalm drys in pipes.

how or is there any ways i can apply more heat to these pipes to make up for the cool off.
Save
Cancel
Reply
replied to:  leegodfrey
truckie11
Replied to:  I have a lipbalm kettle with stainless steel pipes that get...
Piece of piss mate, I'm guessing that's 160 degrees F right? wrap copper pipe around the stainless steel pipes & run hot water through it on a recirculation system.